Professional concrete repairs Melbourne service and Concrete Resurfacing Melbourne
Our Latest Blog

Types of Concrete Cracks: Which Ones Matter and Which Don’t

Every slab cracks. What you need to know is which types of concrete cracks on your floor are cosmetic, which are slow-moving, and which indicate the slab has lost support or the steel inside is rusting.

Here we cover the six types of cracks that usually turn up on warehouse, factory and commercial floors and the difference between a bad-looking crack and a dangerous one.

Quick Answer
  • Most types of concrete cracks on commercial floors are manageable. Hairline cracks in concrete (less than about 0.3 mm) are typically cosmetic.
  • A crack matters when it widens, when one side sits higher than the other, when its edges break up, or when it runs through a forklift wheel path.
  • Structural cracks in concrete (settlement, overload and rusting reinforcement) need an engineer’s judgement before anyone fills them.
  • AS 2870 is a residential standard. Use its crack bands as a reference point, not a pass mark for a commercial slab.
  • Measure and date every crack you’re unsure about. A reading beats an opinion.

Types of Concrete Cracks

The widths below are practical triage bands built around the AS 2870 floor classes. They aren’t a code limit for commercial slabs.

Crack type Typical width Does it matter under forklift traffic? Action
Plastic shrinkage Under 0.3 mm; shallow, map-like or short random lines Rarely, unless the surface is dusting or flaking Monitor; seal if the surface is dusting
Drying shrinkage 0.3–1 mm; often straight, running off joints Sometimes, it matters once the edges break up Seal or fill with a flexible joint filler; repair edges early
Curling Any width, near joints and slab corners; hollow sound or rocking underfoot Yes – wheels hit the raised edge Repair: stabilise the slab and rebuild the joint edge
Settlement 1–2 mm and growing, usually with a step Yes – steps and voids Call an engineer if over 2 mm or stepped; repair once the cause is fixed
Overload Over 1 mm; full depth, often spalled, in wheel paths or under racking legs Yes Call an engineer
Rust from reinforcing steel Any width; follows a bar line, with rust staining or flaking Yes – loose cover breaks away under wheels Call an engineer, then structural repair

Are Cracks in Concrete Normal?

Yes. Concrete shrinks as it dries, and when something restrains that shrinkage, such as the subgrade, the reinforcement or the rest of the slab, tension builds and the surface cracks. Floors with very large exposed surfaces are particularly prone to early shrinkage cracking. Visible cracks will develop under service loads, which is why design teams are encouraged to agree on crack expectations up front.

Sawn joints exist to give that cracking a planned place to form. But unplanned cracking still occurs on industrial floors, and joints don’t always work as theory suggests.

So, are cracks in concrete normal? Yes. But normal isn’t the same as harmless. What counts is the width, whether the crack is moving, and where it sits.

When to Worry: A Checklist in Millimetres

Whichever of the types of concrete cracks you’re looking at, start by measuring it. Use a crack comparator card or a crack gauge, and mark both ends of the crack with a date. Then check against this list:

  • It’s growing. Even 0.2 mm of change between dated readings means something is still moving.
  • Over 1 mm in a wheel path. Anything wider than 1 mm across an aisle, intersection, or racking footprint should be reviewed.
  • Over 2 mm anywhere. That’s past the “distinct” band in AS 2870’s floor classes.
  • One side is higher. Any step you can feel underfoot counts. Treat 2 mm or more as a repair job.
  • Wide enough for a pencil. If a 2 mm pencil lead slides in, it’s not a hairline.
  • Edges are chipping. Spalling along a crack means wheels are already hitting it.
  • Rust staining or a bar-line crack. A crack that tracks a straight line, with brown staining, points to corroding steel.
  • The slab moves. If panels sound hollow when you drag a chain, or shift when a loaded forklift passes, the support has gone.

Any one of the last four items is a prompt to have the slab assessed. Hairline cracks in concrete that haven’t changed across two or three dated readings can usually be left alone.

What Does AS 2870 Say About Crack Width?

AS 2870-2011 sets requirements for site classification and footing design for single dwellings and townhouses. Its Appendix C classifies damage from foundation movement. For concrete floors, a civil and structural engineer’s report applying that appendix uses these approximate bands:

  • Hairline: under 0.3 mm. Barely visible.
  • Fine: under 1.0 mm. Easy to see, still narrow.
  • Distinct: under 2.0 mm. Obvious, and wide enough to collect dirt and water.

That’s a useful shared vocabulary. But it’s a residential standard, written for houses on reactive soils. A commercial slab carries concentrated racking loads and hard-wheeled traffic that a house slab never sees.

So the types of concrete cracks that are acceptable in a garage may not be acceptable in a distribution centre, and the call belongs to an engineer who knows the slab design and the loads.

Six Types of Concrete Cracks on Commercial Floors

1. Plastic shrinkage: hairline cracks in concrete

These form in the first hours after the pour, when the surface loses water faster than it can be replaced. They’re shallow, and most are hairline. On an established floor, they’ve usually stopped moving years ago. Monitor them, and seal the surface if it’s dusting. If an entire area is crazed and shedding dust, concrete resurfacing services can be a better fix than patching crack by crack, provided the underlying slab is sound.

2. Drying shrinkage

Drying shrinkage carries on for months after the slab hardens, and it’s the most common reason a long, straight crack appears mid-panel or runs off a joint. The amount depends on the water–cement ratio and the aggregate–cement ratio.

Most sit between 0.3 and 1 mm. They matter when the edges start to chip. Fill them with a flexible joint filler, and rebuild any broken edges before they get worse.

3. Curling and rocking joints

Curling happens when the top of the slab dries and shrinks faster than the bottom. This moisture difference lifts the panel edges, leaves a void underneath, and exposes the joint edges to wheel impacts.

The crack itself can be thin. The damage comes from vertical movement. Listen for a hollow sound and feel for a bump as wheels cross. Our guide to joint failure under forklifts covers how it develops. Fixing it means stabilising the slab first, then rebuilding the joint edge.

Structural Cracks in Concrete: Settlement, Overload and Rust

These three are the structural cracks in concrete where the slab’s capacity is in question. Don’t fill them until you know the cause.

4. Settlement

If the ground beneath the slab compacts, washes out, or becomes saturated by a leaking service line, the slab loses support. You’ll see cracks that widen over time, often with a step across them and a hollow sound underneath. Anything over 2 mm, or any crack with a step, needs an engineer to find the cause. Repair a settlement crack before the cause is fixed, and it will reopen.

5. Overload

Overload cracks appear where loads exceed the slab’s design capacity. Heavier forklifts, higher racking and stacked pallets are common triggers. They’re usually wider than 1 mm, run through the full slab depth and often have chipped edges. Look in wheel paths and around racking legs.

6. Rust from reinforcing steel

When steel corrodes, the rust occupies more space than the metal did and splits the concrete cover. This can be caused by carbonation and chloride attack. The cracks follow a bar line, with brown staining and flaking cover. Any crack that tracks a bar line is worth assessing. This one needs structural concrete crack repair: the loose concrete comes out, the steel is cleaned or replaced, and the section is rebuilt.

What Happens Next: Repair at Diverse Floor Restorations

Cracks that need repair, rather than monitoring, are our daily work. Concrete floor crack repair at Diverse Floor Restorations uses epoxy and polyurea materials, with partial-depth and full-depth repairs as needed.

Not sure which of these types of concrete cracks you have? Call us on 0405 511 285 or email us. We’ll identify the crack type, measure it, and tell you plainly whether it’s a monitor, seal, repair or engineer job.

Cost depends on width, depth and access. Our guide to crack repair costs breaks down the factors that drive the price.